Polyimide Tape Technical Data Sheet


The Polyimide Tape Technical Data Sheet compares published silicone, acrylic and ESD-grade values for thickness, peel adhesion, tensile behavior, electrical breakdown and heat exposure. These construction-specific figures are references, not common acceptance limits. Steel adhesion cannot predict removal from every coating; a reflow peak cannot establish continuous service temperature. Confirm edge retention, adhesive traces and electrical suitability on representative samples under actual heating, cooling and handling conditions.
Film Gauge Is Not Finished Thickness
A published silicone grade has 25 um backing and 60-66 um finished thickness. The polyimide tape range includes different adhesive systems. The following table separates grade-specific data.
Grade-Tagged Published Properties
Item | Reference Value | Test / Condition | Notes |
Silicone film / total | 25 / 60-66 um | Published silicone grade | Liner excluded |
Acrylic total thickness | 50-80 um | Published acrylic grades | Acrylic only |
Steel peel, silicone / acrylic | 2.3 N/cm / 2.5-4.0 N/25 mm | Methods incomplete | Not comparable |
Tensile, silicone / acrylic | 45 N/cm / >=115 N/25 mm | Published grades | Widths differ |
Elongation, silicone / acrylic | 35% / >=40% | Published grades | Unconfirmed method |
Electrical breakdown | 6.5-7.5 / >=6.0 kV | Silicone / acrylic | Not operating voltage |
Service / brief heat | 180 / 260 C silicone; 150 / 180 C acrylic | Published grades | Time-specific |
Reflow observation | 10 cycles; 245-250 C peak | Silicone trial on FR4 | Not continuous |
ESD resistance / unwind | 10^6-10^9 ohm/sq / <50 V | Special ESD grade | Separate measurements |
Reproducible Measurements
Test | Checks | Method / Reference | Reason | Request When |
Thickness | Film vs total | ASTM D3652 | Avoid stack-up error | Approval |
180-degree peel | Removal force | ASTM D3330; speed, dwell | Steel differs from FR4 | Masking |
Tensile / elongation | Rupture / stretch | ASTM D3759 | Tearing | Slit strips |
Breakdown / heat / ESD | Failure / charge | ASTM D1000; heat cycle; ESD method | Separate mechanisms | Relevant grades |

Qualification on Actual Substrates
On FR4 or coated metal, record pressure, dwell and cooling. After heating, inspect edge lift, bubbles, shadow, tearing and residue. Use 24 h / 72 h / 7 day peels when relevant.

Failure Signals Before Approval
Data | Too Low | Too High | Failure Risk | Verification |
Peel | Edge lift | Removal difficult | Leakage / transfer | Aged substrate peel |
Thickness | Below design | Fit interference | Clearance mismatch | Film / total gauge |
Heat / ESD | Outside range | Beyond validation | Residue / static | Cycle / charge tests |

Lot and Storage Evidence
Record lot, settings, storage age, moisture, sunlight and transport exposure. Set acceptance limits.
FAQ
Why does finished tape exceed PI film thickness?
Adhesive adds thickness; exclude liners.
Can steel peel predict FR4 removal?
No. Test solder mask and dwell.
Is 260 C a continuous rating?
No. Verify duration, cycles and removal.
Does ESD resistance predict unwind voltage?
No. Test resistance and charge separately.