Blown Hand Stretch Film

80 gauge stretch film
hand stretch film
stretch film pallet
stretch film suppliers
80 gauge stretch film
hand stretch film
stretch film pallet
stretch film suppliers
  • Material: LLDPE-based polyethylene; confirm grade by SKU
  • Process: Blown extrusion
  • Color: Clear; other colors subject to confirmation
  • Gauge options: 60, 70, 80, 90 and 120 gauge (market references)
  • Roll width: 12-18 in (market reference)
  • Roll length and core ID: Confirm by SKU

Blown hand stretch film is produced by extruding polyethylene through a circular die, inflating it into a bubble, and cooling it before winding. Bubble expansion and cooling affect the film’s gauge profile, while resin formulation influences toughness and cling. It is often evaluated for metal parts, timber, and cartons with exposed corners. When choosing hand applied blown stretch wrap, compare puncture resistance, tear propagation, cling, and unwind behavior on the actual load rather than judging by gauge alone.

Stretch wrap production

What Blown Extrusion Changes

Resin blend, bubble expansion, cooling, and winding mean two films at the same gauge can behave differently. Puncture resistance measures penetration resistance; tear propagation describes how an existing cut spreads. An impact result does not replace a tear test. One-side and two-side cling depend on formulation, not simply on blown extrusion. For other manual-roll formats, see the hand stretch film range and roll formats.

Benefits

  • Worth evaluating where exposed edges cause repeated punctures.
  • Cling options help keep film layers and the tail in place.
  • Different gauges suit varied load shapes and handling conditions.
  • Suitable grades may help with rough or irregular loads.

How Can Operators Reduce Film Breaks on Sharp-Corner Loads?

Inspect the break point first. Repeated failures may indicate exposed metal, timber splinters, carton edges, or a nick on the roll edge. Use edge protectors where needed and keep hand tension consistent. If breaks continue, compare another grade under the same wrapping pattern. Pulling less tightly may weaken load restraint. Record the break location and check for loose tails or load movement before changing several variables.

Blown film may be evaluated for loads with rough surfaces or exposed edges, but the actual grade must be tested against the application. For narrow-band grouping of compatible items, see extended core bundling stretch film. Choose the format according to the required coverage area and handling method.

Stretch film roll

Applications

Blown hand pallet wrap is worth testing where contact damage is the main concern:

  • Metal parts with exposed edges.
  • Timber and rough building materials.
  • Sharp-edged cartons and mixed pallet shapes.
  • Irregular industrial loads.

The deciding factor is the film-to-load contact point. For broader load-restraint guidance, see pallet stretch film for load stabilization.

.

Stretch film packaging

Technical Data Sheet (TDS)

External references only, not AOBERIS TAPE specifications. IPG HWII supplies the mechanical data; dimensions come from separate market products.

ParameterPublished reference valueSource / note
Gauge options60, 70, 80, 90, 120 gaugeMarket references; confirm availability
Nominal thickness60 = 15.2 um; 70 = 17.8 um; 80 = 20.3 um; 90 = 22.9 um; 120 = 30.5 umGauge conversion
Roll width12-18 inMarket reference
Roll length1,500 ft on selected productsSeparate market reference
Core ID3.05 in +/- 0.05 inSeparate product reference
Net roll weightTo be confirmedVerify by SKU
80-gauge tensile, MD / TD6200 / 4800 psiIPG HWII; ASTM D882
80-gauge elongation, MD / TD500% / 670%IPG HWII; ASTM D882
80-gauge tear, MD / TD90 / 350 gIPG HWII; ASTM D1922
80-gauge dart impact61 gIPG HWII; ASTM D1709
Pre-stretch at break275%Published manufacturer method
Cling at 200% pre-stretch250 g, in-to-outPublished manufacturer method

The IPG HWII technical data sheet lists the mechanical results. MD means machine direction; TD means transverse direction. Dart impact is not a direct test of puncture on a real pallet.

Blown vs. Cast: Practical Trade-Offs

FactorBlown hand filmCast hand film
Puncture resistanceOften worth evaluating; verify gradeGrade-dependent
Tear propagationTest separatelySome grades perform well
ClarityCommonly hazierCommonly clearer
Unwind noiseOften louderOften quieter
ClingOne-side or two-side optionsOne-side or two-side options
Gauge consistencyDepends on bubble controlDepends on cast-line control

These are general tendencies, not guarantees. Blown may suit higher puncture-risk loads; cast may suit operations prioritizing clarity and quiet unwinding. Compare similar gauges under the same conditions.

Validate the Film on the Actual Load

Record gauge, wrap pattern, tension, cling, and storage temperature. Check punctures, tear growth, loose tails, and load movement. ASTM D882 covers tensile properties, D1922 propagation tear, and D1709 dart impact. For cold storage, test at the target temperature. AOBERIS TAPE should verify thickness tolerance, dimensions, net weight, core ID, cling, and product-specific reports before making guarantees.

Stretch film loading

When Should Blown Hand Stretch Film Be Selected Instead of Cast Film?

Consider blown film when sharp edges, rough materials, or irregular shapes cause recurring punctures. Cast may suit applications where visibility and quiet unwinding matter more. Trial both on representative loads and compare breakage, cling, and stability. A blown hand film stretch wrap grade should match contact risks, not gauge alone.

FAQ

Does blown hand stretch film always outperform cast film?

No. Results depend on formulation, gauge, process control, and test method.

Is one-side cling better than two-side cling?

Neither is universal. One-side cling may reduce unwanted sticking; two-side cling can help layers grip.

Which gauge suits sharp-corner loads?

There is no universal gauge. Check edge shape, wrapping pattern, tension, and trial results.

Can blown hand stretch film be used in cold storage?

Potentially. Verify cling, breakage, and handling at the actual storage temperature.